EFFECT OF CALCINATION TEMPERATURE ON THE PROPERTIES AND CATALYTIC PERFORMANCE OF NICKEL OXIDE IN THE ETHANE OXIDATIVE DEHYDROGENATION REACTION
DOI:
https://doi.org/10.52292/j.laar.2022.809Keywords:
nickel oxide, ethane, etheneAbstract
In this paper, the catalytic behavior of nonstoichiometric nickel oxides was investigated in the ethane oxidative dehydrogenation reaction (ODH). The oxide was obtained by heat treatment in the range 250 – 400°C of β-Ni(OH)2 synthesized by precipitation-oxidation. The structural properties of the catalysts were characterized by XRD, FTIR, UV-vis, and SEM. The selective ODH reaction was quantified by gas chromatography. The samples showed pure NiO cubic structure with different degrees of crystallinity, crystallite size, and specific surface area. The increase of calcination temperature caused an increase in the average crystallite size from 28 Å at 250 °C to 104 Å at 400 °C, whereas the shape of the particles showed no significant differences; pore diameter increased from 35 Å to 69 Å and specific surface area decreased from 245 to 82 m2/g. The test carried out at 240°C showed a decrease in conversion, from 8.75% to 4.25%; the more crystalline samples displayed the highest intrinsic activity with selectivity to ethene close to 60%. No influence of band-gap energy on catalytic properties was observed.
Published
Issue
Section
License
Copyright (c) 2022 Latin American Applied Research - An international journal

This work is licensed under a Creative Commons Attribution-NonCommercial-NoDerivatives 4.0 International License.
Once a paper is accepted for publication, the author is assumed to have transferred its copyright to the Publisher. The Publisher will not, however, put any limitation on the personal freedom of the author to use material from the paper in other publications. From September 2019 it is required that authors explicitly sign a copyright release form before their paper gets published. The Author Copyright Release form can be found here